What are the Causes and Prevention Methods for Positive Tolerance Exceeding on Both Sides of the Maximum Diameter of the Core?

ホーム > FAQ > What are the Causes and Prevention Methods for Positive Tolerance Exceeding on Both Sides of the Maximum Diameter of the Core?

What are the Causes and Prevention Methods for Positive Tolerance Exceeding on Both Sides of the Maximum Diameter of the Core?

微信分享

请复制下面链接,在微信内打开分享
https://www.lstransformer.com/ja/what-are-the-causes-and-prevention-methods-for-positive-tolerance-exceeding-on-both-sides-of-the-maximum-diameter-of-the-core%ef%bc%9f/

What are the Causes and Prevention Methods for Positive Tolerance Exceeding on Both Sides of the Maximum Diameter of the Core?

コンテンツ

1.Cause Analysis

(1) Thickness Deviation During Core Stacking:

During the core stacking process, if the thickness of the laminations in each layer is generally thicker, it will directly result in the overall thickness and diameter of the core exceeding the specified tolerance. This typically occurs due toinconsistencies in lamination thickness during manufacturing or handling, or a lack of effective thickness control during stacking.

 

未定義

(2) Misalignment of Core Laminations:

If the laminations of the core exhibit significant left-right misalignment, it will lead to an irregular geometric shape of the core, causing the measurement of the maximum diameter to exceed the positive tolerance. This misalignment may be caused by inaccurate positioning or improper operation.

未定義

(3)  Inadequate Clamping of the Core:

After the core stacking is completed, if the core is not effectively clamped, it can deform or shift during subsequent processing or testing, thereby affecting measurement results and causing the measurements on both sides to exceed the positive tolerance.

2.Preventive Measures

(1) Strict Control of Core Stacking Thickness:

During core stacking, the thickness of each layer of laminations must be strictly controlled. Typically, the thickness tolerance of each core layer is required to be±0.5mm, and positive tolerance is not allowed to occur simultaneously in three consecutive layers. This can be achieved by regularly calibrating the thickness measuring tools for laminations, optimizing the lamination manufacturing process, and implementing stringent quality control measures during stacking.

 

未定義

(2) Ensuring Symmetry of Core Laminations:

During the core stacking process, strict control over the symmetry of the laminations on both sides of each layer is necessary. Precise positioning devices and alignment tools should be used to ensure that each layer of laminations is accurately aligned toprevent left-right misalignment. This can be accomplished by optimizing the positioning and alignment process of the laminations and regularly checking and adjusting for symmetry.

(3) Adequate Clamping and Improved Binding Process for the Core:

After the core stacking is completed, the core should be adequately clamped immediately to prevent deformation during processing or testing. The accuracy of the core binding process should be improved by using appropriate clamping tools and binding materials, ensuring that the core does not bulge after binding. Regular inspections of the clamping equipment are necessary to ensure its proper functioning, and the binding process should be monitored and adjusted to prevent uneven clamping or looseness.

 

未定義

概要

By implementing the aforementioned measures, the issue of positive tolerance exceeding the measurements on both sides of the core’s maximum diameter can be effectively prevented, ensuring that the geometric dimensions of the core meet design requirements, thereby enhancing the performance and reliability of the transformer.

連絡先

廬山,est。 1975年には中国の専門職の専門メーカーの電力変圧器及び原子炉のための50+る。 主製品 単相トランス、三相絶縁変圧器、電気トランス、物流トランス、ステップの下、信用リスク以外のリスクにつきトランス、低電圧トランス、高電圧トランス、制御トランス、トロイダルトランス、Rコアトランス直流インダクター、AC炉では、フィルタリング炉、負荷炉chokes、フィルタリングの原子炉は、中間体、高周波製品.

当社の電力変圧器及び原子炉に広く使用されて10アプリケーション:高速鉄道、建設機械、再生可能エネルギー、ロボット、医療機器、炭鉱爆発の防止、励起システム、真空焼結(炉)、中央エアコンがあります。